Pipa A671 CC65
Nov 21, 2023
Komposisi Kimia Pipa A671 CC65
| Spesifikasi | Kualitas baja | Komposisi kimia | Perkataan | |||||
| C | Ya | M N | P | S | Ti | |||
| Pipa untuk layanan tekanan ASTM A671, A672 |
-/A45 | -/0.17 | - | 0.98 | 0.035 | 0.035 | - | A671/ A672 |
| -/A50 | -/0.22 | - | ||||||
| CA55/A55 | 0.28 | - | ||||||
| -/B55 | -/0.20 | 0.13 ~0.45 |
||||||
| CB60/B60 | 0.24 | |||||||
| CB65/B65 | 0.28 | |||||||
| CB70/C70 | 0.31 | 1.30 | ||||||
| -/C55 | -/0.18 | 0.55 ~0.98 |
||||||
| CC60/C60 | 0.21 | |||||||
| CC65/C65 | 0.24 | 0.79 ~1.30 |
||||||
| CC70/C70 | 0.27 | |||||||
Sifat Mekanik Pipa A671 CC65
| Produk | Kualitas baja | KOMPOSISI MEKANIK LOGAM DASAR | Kekuatan tarik titik pengelasan (N/mm2) | Perkataan | |||
| Titik hasil (N/mm2) | Kekuatan Tarik (N/mm2) | Potongan Tes | Perpanjangan (%) | ||||
| Pipa untuk layanan tekanan ASTM A671, A672 | -/A45 | -/165 | -/310~450 | - | -/30 | -/310~450 | A671/ A672 |
| -/A50 | -/185 | -/345~485 | -/28 | -/345~485 | |||
| CA55/A55 | 205 | 380~515 | 27 | 380~515 | |||
| -/B55 | -/205 | -/380~515 | -/27 | -/380~515 | |||
| CB60/B60 | 220 | 415~550 | 25 | 415~550 | |||
| CB65/B65 | 240 | 450~585 | 23 | 450~585 | |||
| CB70/B70 | 260 | 485~620 | 21 | 485~620 | |||
| -/C55 | -/205 | -/380~515 | -/27 | -/380~515 | |||
| CC60/C60 | 220 | 415~550 | 25 | 415~550 | |||
| CC65/C65 | 240 | 450~585 | 23 | 450~585 | |||
| CC70/C70 | 260 | 485~620 | 21 | 485~620 | |||

Pengepakan Pipa A671 CC65
Pipa A671 CC65 dimasukkan ke dalam kantong plastik satu per satu, potongannya dibungkus dengan bahan kedap air, dibundel dengan tali nilon. Label yang jelas ditandai di bagian luar kemasan untuk memudahkan identifikasi kuantitas dan ID produk. Kehati-hatian diberikan selama pengoperasian dan transportasi