ASME SA213 T91 Tabung Boiler Baja Paduan Mulus

Oct 13, 2023

ASME SA213 T91 Tabung Boiler Baja Paduan Mulus

 

Bahan Setara Tabung ASTM A213 T91

ASTM KERIUHAN JIS GB
P91 X10CrMoVNNb91 STBA 26 10Cr9Mo1VNbN

Komposisi Kimia ASTM A213 T91

Nilai C M N P, Kurang dari atau sama dengan S, Kurang dari atau sama dengan Ya Kr Mo
T91 0.05–0.15 0.30–0.60 0.025 0.025 0.50–1.00 2.65–3.35 0.80–1.06

Sifat Mekanik ASTM A213 T91

Bahan Kekuatan hasilReH/Rp0,2 N/mm² mnt Kekuatan tarikRm N/mm² Perpanjangan A% min
T91 220Mpa 415Mpa 30

ASME SA213 T91 Seamless Alloy Steel Boiler Tube

Kisaran ukuran tabung ASTM A213

NPS, inci Diameter Luar (mm) Ketebalan Dinding (mm) Maks. Panjang (M)
1/8 10,3 1,24; 1,73; 2,40 12
1/4 13,7 1,65; 2,24; 3,02  
3/8 17,1 1,65; 2,31; 3,20  
1/2 21,3 1,65; 2,11; 2,77; 3,73  
3/4 26,7 1,65; 2,11; 2,87; 3,91  
1 33,4 1,65; 2,77; 3,38; 4,55 10
1.25 42,4 1,65; 2,77; 3,56; 4,85  
1.5 48,3 2,77; 3,68; 5,08  
2 60,3 3,91; 5,54 7
2.5 73,0 5,16; 7,01

ASME SA213 T91 Seamless Alloy Steel Boiler Tubes