Pipa ASTM A178 tersedia
Sep 07, 2023
Deskripsi Produk
Pipa ASTM A178 adalah pipa ERW baja karbon dan karbon mangan yang digunakan pada boiler, cerobong boiler, dan superheater. ASTM A178 memiliki A178 grade A (baja karbon rendah), A178 grade C (baja karbon sedang), dan A178 grade D (baja karbon). ) baja mangan).
Pipa ASTM A178 dalam Spesifikasi Stok
|
Nama Produk |
Pipa ASTM A178 tersedia |
|
Diameter luar |
14mm-720mm |
|
Bahan |
GB10#,20,#35,40#,45#,16Mn,35Mn2 ,40Mn2,45Mn2,35SiMn,42SiMn,40Cr, Q345,Q355, Q390,20MnG,25MnG,15MoG,20MoG,12CrMoG,15CrMoG,12Cr2MoG,12 Cr1MoVG, 10MoWVNb ,12CrMo,15CrMo,1Cr5Mo,12Cr2Mo,37Mo,30CrMo 35CrMo,34CrMo4,T/P5,T/P9,DZ40,DZ50,DZ55,DZ60,STM-R780 ASTM 1010,1012,1020,1035,1045 ,4130,4140,A53 Gr.A,A53 Gr.B,A53M,A36,A106 Gr.A/Gr.B EN P195/235/265GH,16Mo3,13CrMo4-5,13CrMo9-10,15NiCuMoNb5-6-4 St35.8, St45.8,15Mo3,13CrMo44,10CrMo910 API 5L Gr.B |
|
Standar |
GB3094,8162,8163,3639,3087,6479,5310,9948,6479,17396 ,GB/T 17396 ,Q/OHAD010-1998 ,YB/T 5052 Q/OHAD006-2009, YB/T 5035 Q/OHAD001-1997, Q/OHAD015-2008, Q/OHAD002-2010 ASTM A53, A179,A192, A106,ASTM A36,A519, A213,A335 ASEM SA106/SA192/SA209/SA210/SA213/SA335 JISSTPG370,STPT370,STB240 DIN 17175/2391-2 EN 10216/10210 API 5L ............ |
|
Standar toleransi harian |
od: +-1%, berat: +-10% |
|
Memeriksa |
ISO BV SGS SVG |
|
Kemasan |
Pengepakan kelayakan laut standar atau sesuai kebutuhan. |
|
MOQ |
5 metrik ton, pesanan sampel diterima |
|
Waktu pengiriman |
7-10 hari kerja setelah diterimanya setoran atau letter of credit |
|
Cara Pembayaran |
30%TT+70%TT / LC Dll |
|
Menggambarkan |
Permukaan: dicat, dilapisi PE, galvanis |
|
Aplikasi |
1. Pipa transmisi fluida bertekanan sedang dan rendah 2. Casingnya |
|
Keuntungan |
1. Harga wajar, kualitas bagus 2. Persediaan yang cukup, pengiriman cepat |

| Nilai | Karbon | mangan | Fosfor | Sulfur | Silikon |
|---|---|---|---|---|---|
| ASTM A178 Gr A | 0.06% - 0.18% | 0.27% - 0.63% | 0,035% Maks | 0,035% Maks | - |
| ASTM A178 GrC | 0,35% Maks | 0,80% Maks | 0,035% Maks | 0,035% Maks | - |
| ASTM A178 Gr D | 0.27% Maks | 1.00% - 1.50% | 0,30% Maks | 0.015% Maks | 0.10% Min |
| Nilai | P # | Daya tarik | Menghasilkan | Kekerasan Maks | Periksa Inventaris |
|---|---|---|---|---|---|
| ASTM A178 Gr A / SA178A | P 1 | ksi : 47 MPa : 325 | ksi : 26 MPa : 180 | 77HRB (Rockwell B) | A178 Gr A Persediaan |
| ASTM A178 Gr C / SA178C | P 1 | ksi : 60 MPa : 415 | ksi : 37 MPa : 255 | 79HRB (Rockwell B) | Inventarisasi A178 Gr C |
| ASTM A178 GrD/SA178D | P 1 | ksi : 70 MPa : 485 | ksi : 40 MPa : 275 | 77HRB (Rockwell B) | A178 Gr D Persediaan |