Apa's The Perbedaan Antara API 5L Gr.B And A106 Gr.B?

Oct 25, 2023

API5L GR. B Pipes come from API Spec 5L Specification for Line Pipe with the application of gas, water and oil transportation. Standard Line Pipe has grade designation A and B. API 5L Grade b pipe can be two of API 5L product service level (PSL), that's is API 5L Gr.B PSL1 and API 5L Gr. B PSL2.
ASTM A106 (S% 2fA 106) pipa adalah standar spesifikasi untuk mulus karbon baja pipa untuk suhu tinggi dan tekanan layanan. ASTM A106 pipa termasuk tiga nilai% 3a ASTM A106 Kelas A% 2c ASTM A106 Kelas B, ASTM A106 Grade C. ASTM A106 grade B Pipe is used in power plants, boilers, petrochemical plants, oil and gas refineries, and ships where the piping must transport fluids and gases that exhibit high pressures and temperature. API 5L Gr.b and A106 Gr.b are both carbon steel that is used in oil and gas transportation. Both of them can be welded, but the most of A106 Gr. B pipe adalah mulus. Di sini adalah beberapa kecil detail tentang A106 kelas B dan API 5L Gr.

info-750-750

Standar

C maks %

Mn maks%

S maks %

Si menit % 25

Cr maks %

Cu maks %

A106 Gr. B

0.30

0.29-1.06

0.035

0.10

0.40

0.40

API 5L Gr.B/L245

0.28

1.20

0.030

/

0.50

0.50

Tarik Persyaratan

Standar

Hasil Kekuatan Mpa

Perpanjangan %

A106 Gr. B

Lebih Besar dari atau sama ke 415

Lebih Besar dari atau sama ke 240

20

API 5L Gr.B/L245

Lebih Besar dari atau sama ke 415

Lebih besar dari atau sama ke 245

23

 


sejak nya pendirian,alwaws adhere to the market-oriented. customer-orientedquality as the lifeblood of the company, good faith as the basis of corporategovernance, adhere to the serious rigorous enterprising, continuous development andgrowth of the principle, in the industry to establish a solid sales service system.

info-800-640