Tabung boiler mulus baja paduan, SA210 gr. Al
Mar 28, 2025
Tabung Tabung Boiler China Pabrik Gnee Grosir Paduan Baja Tabung Seamless, Sa210 AL Tube Boiler, Permukaan Oli Anti-Rust, OD 38.1 mm x Ketebalan 3,66 mm.
Jenis:Tabung boiler mulus baja paduan.
Bahan:SA210 GR.A1.
Perlakuan panas: dinormalisasi.
Permukaan: Minyak anti-rust.
OD: 38.1 mm.
Ketebalan: 3,66 mm.