Pipa Mulus ASTM A335 P5

Apr 02, 2024

Spesifikasi Pipa Mulus Baja Paduan A335 P5

Pipa Chrome Moly: ASTM A335 / ASME SA335 Kelas P5
Jenis fabrikasi: Pipa Baja Mulus
Konten Chrome 4.00 % hingga 6.00%, Molibdenum 0.45 hingga 0.65%.
Rentang Pasokan: 1/2" hingga 36" DN25 hingga DN900
Ketebalan dinding hingga SCH 160
Panjang: SRL, DRL, Panjang Tetap
Perawatan permukaan: Dipoles, Dilapisi 3LPE atau FBE

Data Pipa Mulus ASTM A335 P5

Jadwal Pipa Tekanan Tinggi ASME SA 335 Grade P5

OD x Tebal (mm) OD x Tebal (mm) OD x Tebal (mm)
38.1 x 3.2 57.0 x 4.9 76.2 x 4.0
38.1 x 4.0 57.0 x 6.3 76.2 x 5.0
38.1 x 6.3 57.0 x 7.9 76.2 x 6.3
42.4 x 3.2 60.3 x 3.2 82.5 x 4.5
42.4 x 4.0 60.3 x 3.6 88.9 x 3.2
44.5 x 3.2 60.3 x 5.0 88.9 x 3.6
44.5 x 6.3 63.5 x 3.2 88.9 x 4.0
48.3 x 3.2 63.5 x 3.6 101.6 x 3.6
48.3 x 3.6 63.5 x 4.0 101.6 x 4.5
50.8 x 4.5 63.5 x 6.3 101.6 x 6.3
51.0 x 3.2 63.5 x 7.9 114.3 x 3.6
51.0 x 3.6 70.0 x 3.2 114.3 x 5.0
51.0 x 6.3 70.0 x 3.6 139.7 x 4.0
57.0 x 3.2 70.0 x 6.3 139.7 x 5.0
57.0 x 3.6 76.2 x 3.6 139.7 x 6.3

p5 Bagan Ketebalan Pipa Baja Paduan

NPS [DN] Penunjuk Toleransi, % dari Ditentukan
Lebih Di bawah
1/8 hingga 2 1/2 [6 hingga 65] termasuk, semua rasio t/D 20.0% 12.5%
Di atas 2 1/2 [65], t/D < atau=5% 22.5% 12.5%
Di atas 2 1/2 [65], t/D > 5% 15.0% 12.5%
(t=Ketebalan Dinding yang Ditentukan; D=Diameter Luar yang Ditentukan)

Bagan Komposisi Pipa Las ASTM A335 P5

Baja Paduan P5 C Kr S Ya M N Mo P
0.05 – 0.15 1.00 – 1.50 0,025 maks 0.50 – 1.00 0.30 – 0.60 0.44 – 0.65 0,025 maks

Bagan Sifat Mekanik Pipa P5 Kelas Baja Paduan

Kekuatan Tarik, MPa Kekuatan Hasil, MPa Pemanjangan
415 menit 205 menit 30 menit

ASME SA335 Alloy PipeSA335 P5 High-Pressure Steel Pipe